| Element | Weight (%) | Specification Notes |
|---|---|---|
| Beryllium (Be) | 1.80 - 2.00 | Primary age‑hardening element; gamma‑phase precipitation generates up to 200 ksi tensile strength |
| Cobalt (Co) | 0.20 min - 0.30 max | Grain refiner; controls beryllide particle size during aging |
| Nickel + Cobalt (Ni+Co) | ≥0.20 | Minimum content ensures consistent age‑hardening kinetics |
| Nickel + Cobalt + Iron (Ni+Co+Fe) | ≤0.60 | Upper bound restricts intermetallic formation that reduces ductility |
| Lead (Pb) | ≤0.01 (C17200, RoHS compliant); 0.20-0.60 (C17300 leaded variant) | Ultra‑low lead composition for RoHS‑compliant markets |
| Copper (Cu) | Remainder (≥97.5% min) | High‑purity matrix provides 22-28% IACS baseline conductivity |
| Temper Designation | Diameter or Cross‑Section | Tensile Strength (ksi / MPa) | Yield Strength 0.2% (ksi / MPa) | Hardness | Elongation (%) |
|---|---|---|---|---|---|
| TB00 (A) -- Solution Annealed | All sizes | 60-85 / 414-586 | 20 min / 138 min | B45-85 | ≥20 |
| TD04 (H) -- Hard Drawn | Up to 3/8″ / 9.5 mm incl. | 90-130 / 620-896 | 75 / 517 | B88-103 | 8 |
| TD04 (H) -- Hard Drawn | Over 3/8″ to 1″ / 9.5-25 mm | 90-125 / 620-862 | 75 / 517 | B88-102 | 8 |
| TD04 (H) -- Hard Drawn | Over 1″ to 3″ / 25-76 mm | 85-120 / 586-827 | 75 / 517 | B88-101 | 8 |
| TF00 (AT) -- Mill‑Hardened (Aged) | Up to 3″ / 76 mm incl. | 150-190 / 1034-1310 | 125 / 862 | C32-39 | 4 |
| TH04 (HT) -- Peak Aged | Up to 3/8″ / 9.5 mm incl. | 170-210 / 1172-1448 | 145 / 1000 | C35-41 | 4 |
| TH04 (HT) -- Peak Aged | Over 3/8″ to 1″ / 9.5-25 mm | 170-210 / 1172-1448 | 145 / 1000 | C35-41 | 2 |
| TH04 (HT) -- Peak Aged | Over 1″ to 3″ / 25-76 mm | 165-200 / 1138-1379 | 135 / 931 | C34-39 | 2 |
| Property | Metric Value | Imperial Value | Condition |
|---|---|---|---|
| Density | 8.25-8.36 g/cm³ | 0.298-0.302 lb/in³ | Age‑hardened (~4% increase vs. solution‑annealed) |
| Melting Range | 870-980 °C | 1598-1796 °F | Solidus-liquidus |
| Electrical Conductivity | 22-28% IACS | 0.129 MS/cm at 20°C | Minimum 22% in peak‑aged HT/TH04 temper |
| Electrical Resistivity | 6.1-7.8 μΩ*cm | 37-47 Ω*cmil/ft | Corresponding to conductivity range |
| Thermal Conductivity | 105-135 W/m*K | 62-78 BTU/(ft*hr*°F) | @ 20°C aged condition |
| CTE (20-200°C) | 16.7-17.8 * 10⁻⁶ /°C | 9.9 * 10⁻⁶ /°F (68-572°F) | Low hysteresis for thermal cycling stability |
| Specific Heat Capacity | 0.42 kJ/kg*K | 0.10 BTU/lb*°F | @ 20°C |
| Magnetic Permeability (µᵣ) | <1.01 | -- | Non‑magnetic across all tempers |
| Region | Key Industries | Application Drivers for Beryllium Copper Rod |
|---|---|---|
| North America & Europe | Aerospace, EV manufacturing, defense | AMS 4533 certification for landing gear bushings and instrument housings; RWMA Class IV resistance welding electrodes; IATF 16949 compliance for EV battery contactor shafts |
| Middle East & Africa | Oil & gas, petrochemical, mining | Downhole MWD/LWD pressure housings, drill bit bearings, non-sparking safety tools; NACE MR0175 sour‑gas compliance for H₂S environments |
| South & Southeast Asia | Industrial tooling, automotive connectors, electronics | Plastic injection mold cores for high‑volume consumer goods; JNPT port logistics (India) and ASEAN tariff benefits; high‑cycle relay blades |
| South America | Mining, heavy equipment, oil & gas | Wear plates and non‑sparking pump shafts for acidic mine water (pH 2-4); Mercosur origin documentation for intra‑bloc tariff reduction |
| Global Maritime | Marine propulsion, offshore platforms | Propeller shaft bushings, valve stems, subsea actuator rods; zero hydrogen embrittlement susceptibility; ABS/DNV certifications available |
| MOQ: | 5kg |
| Price: | USD 30-50/kg |
| Standard Packaging: | Carton, Plywood pallet, Plywood box |
| Delivery Period: | 20 days |
| Payment Method: | L/C,T/T |
| Supply Capacity: | 10 tons/month |
| Element | Weight (%) | Specification Notes |
|---|---|---|
| Beryllium (Be) | 1.80 - 2.00 | Primary age‑hardening element; gamma‑phase precipitation generates up to 200 ksi tensile strength |
| Cobalt (Co) | 0.20 min - 0.30 max | Grain refiner; controls beryllide particle size during aging |
| Nickel + Cobalt (Ni+Co) | ≥0.20 | Minimum content ensures consistent age‑hardening kinetics |
| Nickel + Cobalt + Iron (Ni+Co+Fe) | ≤0.60 | Upper bound restricts intermetallic formation that reduces ductility |
| Lead (Pb) | ≤0.01 (C17200, RoHS compliant); 0.20-0.60 (C17300 leaded variant) | Ultra‑low lead composition for RoHS‑compliant markets |
| Copper (Cu) | Remainder (≥97.5% min) | High‑purity matrix provides 22-28% IACS baseline conductivity |
| Temper Designation | Diameter or Cross‑Section | Tensile Strength (ksi / MPa) | Yield Strength 0.2% (ksi / MPa) | Hardness | Elongation (%) |
|---|---|---|---|---|---|
| TB00 (A) -- Solution Annealed | All sizes | 60-85 / 414-586 | 20 min / 138 min | B45-85 | ≥20 |
| TD04 (H) -- Hard Drawn | Up to 3/8″ / 9.5 mm incl. | 90-130 / 620-896 | 75 / 517 | B88-103 | 8 |
| TD04 (H) -- Hard Drawn | Over 3/8″ to 1″ / 9.5-25 mm | 90-125 / 620-862 | 75 / 517 | B88-102 | 8 |
| TD04 (H) -- Hard Drawn | Over 1″ to 3″ / 25-76 mm | 85-120 / 586-827 | 75 / 517 | B88-101 | 8 |
| TF00 (AT) -- Mill‑Hardened (Aged) | Up to 3″ / 76 mm incl. | 150-190 / 1034-1310 | 125 / 862 | C32-39 | 4 |
| TH04 (HT) -- Peak Aged | Up to 3/8″ / 9.5 mm incl. | 170-210 / 1172-1448 | 145 / 1000 | C35-41 | 4 |
| TH04 (HT) -- Peak Aged | Over 3/8″ to 1″ / 9.5-25 mm | 170-210 / 1172-1448 | 145 / 1000 | C35-41 | 2 |
| TH04 (HT) -- Peak Aged | Over 1″ to 3″ / 25-76 mm | 165-200 / 1138-1379 | 135 / 931 | C34-39 | 2 |
| Property | Metric Value | Imperial Value | Condition |
|---|---|---|---|
| Density | 8.25-8.36 g/cm³ | 0.298-0.302 lb/in³ | Age‑hardened (~4% increase vs. solution‑annealed) |
| Melting Range | 870-980 °C | 1598-1796 °F | Solidus-liquidus |
| Electrical Conductivity | 22-28% IACS | 0.129 MS/cm at 20°C | Minimum 22% in peak‑aged HT/TH04 temper |
| Electrical Resistivity | 6.1-7.8 μΩ*cm | 37-47 Ω*cmil/ft | Corresponding to conductivity range |
| Thermal Conductivity | 105-135 W/m*K | 62-78 BTU/(ft*hr*°F) | @ 20°C aged condition |
| CTE (20-200°C) | 16.7-17.8 * 10⁻⁶ /°C | 9.9 * 10⁻⁶ /°F (68-572°F) | Low hysteresis for thermal cycling stability |
| Specific Heat Capacity | 0.42 kJ/kg*K | 0.10 BTU/lb*°F | @ 20°C |
| Magnetic Permeability (µᵣ) | <1.01 | -- | Non‑magnetic across all tempers |
| Region | Key Industries | Application Drivers for Beryllium Copper Rod |
|---|---|---|
| North America & Europe | Aerospace, EV manufacturing, defense | AMS 4533 certification for landing gear bushings and instrument housings; RWMA Class IV resistance welding electrodes; IATF 16949 compliance for EV battery contactor shafts |
| Middle East & Africa | Oil & gas, petrochemical, mining | Downhole MWD/LWD pressure housings, drill bit bearings, non-sparking safety tools; NACE MR0175 sour‑gas compliance for H₂S environments |
| South & Southeast Asia | Industrial tooling, automotive connectors, electronics | Plastic injection mold cores for high‑volume consumer goods; JNPT port logistics (India) and ASEAN tariff benefits; high‑cycle relay blades |
| South America | Mining, heavy equipment, oil & gas | Wear plates and non‑sparking pump shafts for acidic mine water (pH 2-4); Mercosur origin documentation for intra‑bloc tariff reduction |
| Global Maritime | Marine propulsion, offshore platforms | Propeller shaft bushings, valve stems, subsea actuator rods; zero hydrogen embrittlement susceptibility; ABS/DNV certifications available |